美国开发出最小分辨率可达0.5埃的电子显微镜
发布时间:2007-09-22    来源:网络   阅读次数:1544 分享到:

     美国能源部国家实验室、FEI公司以及CEOS GmbH公司联合开发出一套具有突破性意义的电子显微镜——最小分辨率可达0.5埃。 这项研究得到美国能源部基础能源科学办公室TEAM Project (Transmission Electron Aberration-corrected Microscope)计划支持。

    此款TEAM电子显微镜引入了最新的像差修正技术(aberration correctors),能够在一台设备上得到更高稳定性的透射电镜(TEM)与扫描透射电镜(STEM)图像,研究人员可以直接观察到物质原子堆积情况。

    随着纳米研究的深入,电子显微镜所发挥作用越来越重要.

相关英文:

TEAM PROJECT ACHIEVES MICROSCOPY BREAKTHROUGH 0.5 Angstrom Imaging Milestone Reveals the Smallest Details Ever Seen by Electron Microscopy HILLSBORO, Ore./September 6, 2007 The highest-resolution images ever seen in (S)TEM electron microscopy have been recorded using a new instrument developed jointly by U.S. Department of Energy national laboratories, FEI Company (Nasdaq: FEIC) and CEOS GmbH, in Heidelberg, Germany. This breakthrough in electron microscopy -- with 0.5 ?ngstr?m and below performance -- is a result of The TEAM Project (Transmission Electron Aberration-corrected Microscope) supported by the U.S. Department of Energy’s Office of Science Basic Energy Sciences. One-half ?ngstr?m is one one-billionth of five centimeters. To put that in perspective, the DNA helix is approximately 20 ?ngstr?ms in diameter, a carbon atom is around two ?ngstr?ms. The width of an average strand of human hair ranges from 500,000 to one million ?ngstr?ms. Electron microscopes can be used to observe fine details of the inner structure of materials.
 The ability to characterize the atomic-scale structure, chemistry, and dynamics of individual nanostructures makes this type of microscope a very powerful tool for scientists in all disciplines. With the extraordinary ‘vision’ of the special TEAM microscope it will become possible to study how atoms combine to form materials, how materials grow and how they respond to a variety of external factors. These constitute many of the most practical things that science needs to know about materials and will improve designs for everything from better, lighter, more efficient automobiles, to stronger buildings and new ways of harvesting energy. The landmark performance was achieved using both TEM (transmission electron microscope) and STEM (scanning transmission electron microscope) imaging -- two methods used by researchers to directly view the basic building blocks of all matter.
The unprecedented performance recorded in these two imaging modes has been achieved on a single instrument developed by FEI Company -- using Titan? S/TEM technology --equipped with two CEOS-designed spherical aberration correctors, dramatically improving the microscope’s imaging and other abilities. The special TEAM microscope is the result of a series of new technology breakthroughs, providing for higher stability than previously possible and incorporating the newly designed aberration correctors. TEM images obtained show an information transfer down to 0.5 ?ngstr?m. In STEM mode, frequencies better than 0.5 ?ngstr?m were recorded. Further details and examples of the benefits for nanoscience and research can be found on the TEAM website:
http://ncem.lbl.gov/TEAM-project/. "This is a great achievement in electron microscope development,” said Ulrich Dahmen, TEAM project Director and Director of Lawrence Berkeley National Laboratory’s National Center for Electron Microscopy. “As the first big collaborative project for the microscopy community, TEAM set ambitious goals. To have reached the 0.5 ?ngstr?m goal early in the project is a significant milestone for the collaboration, and a validation of the Department of Energy's investment in the development of world-leading scientific instrumentation. Now we look forward to transferring the remarkable performance of the TEAM microscope into a tool for exploration of atomic structure in the nanoworld.” “As the limits of nanotechnology are expanded ever further, FEI is committed to continually breaking through the most challenging barriers of imaging and analysis,” commented Don Kania, FEI’s president and CEO. “The TEAM collaboration’s success underscores the strength of FEI’s technology and FEI’s commitment to innovation. This achievement is an important breakthrough in our mission to create tools and applications that deliver new, ultra-high resolution information at the extremes of performance.” Max Haider, CEO of CEOS GmbH, also commented on the results of the collaboration. “The performance achieved by the TEAM microscope sets a landmark in the history of high resolution TEM and STEM imaging.
 